Small 2021, 17(39), 2102088

Applications of Atomic Layer Deposition in Design of Systems for Energy Conversion

There is a huge demand for clean energy conversion in all industries. The clean energy production processes include electrocatalytic and photocatalytic conversion of water to hydrogen, carbon dioxide reduction, nitrogen conversion to ammonia, and oxygen reduction reaction and require novel cheap and efficient photo- and electrocatalysts and their scalable methods of fabrication. Atomic layer deposition is a thin film deposition method that allows to deposit thin layers of catalysts on virtually any surface of any shape, size, and porosity in an even and easy to control manner. Here the state of the art in applications of atomic layer deposition in the clean energy production and the opportunities it represents for the whole field of the photo- and electrocatalysis for a sustainable future are reviewed.